隧道初支变形原因分析及有效综合处理措施

2017-05-11 20:19:25魏欣
价值工程 2017年14期

魏欣

摘要: 四川省汶马高速公路米亚罗3号隧道右线K163+970~+905段隧道围岩具有膨胀性,施工期间多次出现初期支护混凝土环向、纵向变形开裂,表层起皮掉块,初支钢架严重变形,部分初期支护严重侵限等多种质量问题。文章重点阐述了隧道产生初支变形的分析过程及采取的针对性综合整治措施。

Abstract: The surrounding rock of the K163 + 970 ~ + 905 tunnel on the right side of Miyaluo No.3 tunnel of Wenma Expressway in Sichuan Province has expansive properties. During the construction period, many quality problems occurred, such as circumferential and longitudinal deformation and cracking of initial supporting concrete, surface peeling off, early support steel frame serious deformation, part of the initial support serious damage and so on. This paper focuses on the analysis process of the initial support deformation of the tunnel and the comprehensive measures to be taken.

關键词: 公路隧道;膨胀性围岩;初支变形;整治措施

Key words: highway tunnel;expansive surrounding rock;initial branch deformation;remediation measures

中图分类号:U459.2 文献标识码:A 文章编号:1006-4311(2017)14-0136-03

0 引言

四川省汶马高速公路米亚罗3号隧道为左右线分离式隧道,隧道间距为25~40m,右线起讫里程K162+723~K166+000,长度4277m。采用双曲线半圆拱的断面形式,隧道净宽10.9m,隧道净高7.2m。

施工期间米亚罗3号隧道右线K163+970~+910段洞顶发生初期支护砼纵向开裂、掉块现象,下边墙连接板处初期支护挤出下沉开裂,边墙初期支护墙面不均匀挤出,拱顶渗水。钢架变形超限。部分拱顶初期支护拱架形成褶曲,受力结构破坏等隧道病害。

此段原设计围岩为Ⅳ级,采用Z4型衬砌支护,超前支护采用?准22药卷锚杆支护。

经过分析研究病害产生的原因,并采取针对性的综合有效处理措施和施工方法,完成了此段隧道的变形整治。现将整治此段隧道的技术措施及特殊工艺及方法作如下介绍。

1 工程地质概况

此段变形隧道由大里程向小里程方向掘进。K163+950里程的地质情况较为典型:

掌子面揭露围岩以泥质千枚岩、板岩互层夹变质砂岩组成。掌子面左部和中部灰色薄层板岩、泥质千枚岩互层,挤压强烈,富含石英脉岩层紊乱极破碎,已软化泥化,围岩自稳能力极差,导致超挖严重;……

登录APP查看全文