铝合金燃油箱焊接缺陷产生原因及控制措施

2018-10-21 16:10:50张友龙袁文强芮凯朱成燕
汽车实用技术 2018年12期
关键词:焊接控制措施

张友龙 袁文强 芮凯 朱成燕

摘 要:随着重型卡车对轻量化的要求越来越高,铝合金材料在重卡底盘上的应用也越来越广泛,铝合金燃油箱作为重卡底盘的典型轻量化部件,在批量生产过程中存在焊接气孔、裂缝、未熔合等缺陷,通过对焊缝焊接缺陷、焊缝特征的分析对铝合金油箱焊接缺陷产生原因进行论述并提出预防措施。

关键词:铝合金燃油箱;焊接;控制措施

中图分类号:U466 文献标识码:B 文章编号:1671-7988(2018)12-129-03

Abstract: With the increasing demand for light weight of heavy trucks, the application of aluminum alloy on heavy truck chassis is more and more extensive. As a typical lightweight component of heavy truck chassis, aluminum alloy fuel tank has defects such as porosity, cracks, and incomplete fusion in batch production.Through the analysis of weld defects and weld characteristics, the causes of welding defects of aluminum alloy fuel tanks are discussed and preventive measures are put forward.

Keywords: Aluminum alloy fuel tank; welding; control measures

CLC NO.: U466 Document Code: B Article ID: 1671-7988(2018)12-129-03

1 铝合金油箱概述

铝合金燃油箱具有重量轻、外表美观、耐腐蚀性好、制造环保、清洁度高等优点。随着重卡市场对底盘轻量化要求的提高,诸如铝合金燃油箱等轻量化零部件的应用也越来越广泛。

铝合金燃油箱主要由端盖、隔板、本体、加油管等零件组成(如图1),通常本体与端盖之间通过焊接结构连接(如2),隔板与本体之间采用点焊、角焊或卡锁连接(如图3)。

铝合金燃油箱焊接通常采用MIG焊(融化极惰性气体保护焊)或TIG焊(钨极惰性气体保护焊)。MIG焊和TIG焊均采用氩气作为保护气体,保证焊接时金属不被氧化。因TIG焊接钨极的费用较高,目前铝合金燃油箱多采用MIG焊接。

2 铝合金燃油箱焊接常见缺陷产生原因及预防措施

铝合金燃油箱焊缝主要集中在:1)端盖与本体连接处(如图2);2)本体自身连接处(如图4);3)底部放油塞处(如图5)。端盖与本体连接处焊缝为环焊缝其主要特征为:1)焊缝较长(一般超过1000mm);2)为封闭式焊缝;3)焊接形状不规则,且受制造误差影响较大。本体连接处焊缝为直焊缝其主要特征为:1)焊缝平直长;……

登录APP查看全文

猜你喜欢
焊接控制措施
给排水工程招投标阶段中的造价控制措施
建筑安装工程预结算造价控制措施
土木工程施工的质量控制措施初探
大型公司财务预算与控制措施探讨
土木建筑施工质量控制措施探讨
浅谈桥梁工程焊接质量管理的研究
CO2气体保护焊在设备制造焊接中的应用
科技视界(2016年22期)2016-10-18 15:39:28
带压堵漏技术在检修中的应用
科技视界(2016年21期)2016-10-17 19:54:05
钢结构焊接中存在问题原因分析与预防研究
企业导报(2016年11期)2016-06-16 15:47:07
铝合金构件焊接变形研究及焊接工艺优化
企业导报(2016年8期)2016-05-31 18:40:49