310S不锈钢反应器失效原因分析

2020-09-09 07:24:45刘晓华廖晓玲孙琪
当代化工 2020年8期
关键词:不锈钢裂纹分析

刘晓华 廖晓玲 孙琪

摘      要:某化工厂S310不锈钢反应器用于氨气加热裂解制氢,投入使用一年后产生贯穿裂纹失效。对设备失效现场、失效管件、工艺流程等进行宏观分析,同时从失效反应器上制取试件,利用金相分析、微观形貌观察、硬度测试、化学成分分析等方法分析反应器筒体裂纹产生的原因。结果表明:反应器处于高温富氢环境下,析出富铬σ相,渗碳体所占比例提高,致使周边组织贫Cr,从而降低了材料的强度,增加了材料的硬度;裂解产生的氢气在反应器内形成富氢环境,使材料发生氢脆反应,进一步降低了材料的性能;安装工艺导致管型反应器应力集中,最终形成贯穿性裂纹并失效。最后针对设备失效原因,提出了相应的防护措施。

关  鍵  词:不锈钢;反应器;腐蚀;裂纹;失效

中图分类号:TQ 050.9      文献标识码: A      文章编号: 1671-0460(2020)08-1719-04

Abstract: S310 stainless steel reactor in a chemical factory was used to produce hydrogen by heating and cracking ammonia gas. After one-year operation, the through crack failure occurred. Macro analysis of equipment failure site, failure pipe fittings, and process flow was carried out, and the test pieces were made from the failed reactor. The reasons of cracking were investigated by phase composition analysis, micro morphology observation, hardness testing and chemical analysis. The results showed that when the reactor was in high temperature and hydrogen rich environment, chromium-rich σ phase was precipitated and the proportion of cementite was increased, resulting in the surrounding tissue to be poor in Cr, reducing the strength of the material and increasing the hardness of the material. The hydrogen produced by cracking formed hydrogen-rich environment in the reactor, which made the material produce hydrogen embrittlement reaction to further reduce the performance of the material. The installation process led to the concentration stress of the tubular reactor, finally causing the through crack and fails. At last, the corresponding protective measures were put forward aiming at the reasons of equipment failure.

Key words: Stainless steel; Reaction vessel; Corrosion; Crackle; Failure

氨分解制氢是一种相对简单高效的化学反应,通常是以800~850 ℃的高温对氨液进行加热直至分解,可得到含25% N2、75% H2的氢氮混合气体。液氨分解制氢在工业上很容易实现,但对分解过程中使用的反应器同时提出了更高的要求。

310S(06Cr25Ci20)不锈钢是奥氏体铬镍不锈钢,是不锈钢中的优质产品,具有良好的耐氧化、耐腐蚀、耐高温性能,可经受住较高负荷[1]。同时奥氏体型不锈钢的化学成分特性是以铬、镍为基础添加钼、钨、铌和钛等元素,其组织为面心立方结构,在高温下有较高的强度和蠕变强度,因而广泛应用于化工行业管道、热交换设备和压力容器等设备中。……

登录APP查看全文

猜你喜欢
不锈钢裂纹分析
裂纹长度对焊接接头裂纹扩展驱动力的影响
隐蔽失效适航要求符合性验证分析
Epidermal growth factor receptor rs17337023 polymorphism in hypertensive gestational diabetic women: A pilot study
80t不锈钢GOR底吹转炉工艺设备改造
山东冶金(2019年1期)2019-03-30 01:35:32
电力系统不平衡分析
电子制作(2018年18期)2018-11-14 01:48:24
不锈钢微钻削的切屑形成与仿真分析
电力系统及其自动化发展趋势分析
OCr18Ni9不锈钢的微小孔钻削
预裂纹混凝土拉压疲劳荷载下裂纹扩展速率
低合金钢焊接裂纹简述