楼康明 高彦斌



摘要:采用室内微型十字板剪切试验对上海两种含水量(w=45.45%,w=34.93%)的饱和软黏土的触变特性进行了研究。结果表明,两种含水量的软黏土重塑扰动后,在触变恢复初期强度增长速度较快,7天后强度恢复速率明显变缓。上海饱和软黏土不是完全触变材料,触变性是其具有高灵敏性的原因之一,其中低水量土样触变性对其灵敏性的贡献明显大于高含水量土样。
Abstract: Thixotropic action of saturated soft clay in Shanghai under two water content (w=45.45%,w=34.93%) were investigated by laboratory mini-vane shear tests. According to the test results, the rate of thixotropic regains in the early period of age-hardening was high, and then slowed down obviously after 7 days. Saturated soft clay in Shanghai is not a complete thixotropic material. Thixotropy is one of the important reasons for its high sensitivity. The thixotropy of low water content soil contributes significantly to its sensitivity than the high water content soil.
关键词:上海;饱和软黏土;触变性;微型十字板;强度
Key words: Shanghai;saturated soft clay;thixotropy;laboratory mini-vane apparatus;strength
中图分类号:TU441.31 文献标识码:A 文章编号:1006-4311(2020)22-0239-03
0 引言
饱和软黏土的触变性是指软黏土受到外界扰动后强度显著降低,在含水量保持不变的情况下土体结构随时间推移逐渐趋于新的平衡,其强度也逐渐增长的现象。土的触变性研究主要包括两方面:①扰动后土体强度降低的特性(即触变软化),是土的灵敏性研究内容之一;②扰动后土体在密度和含水量不变条件下随时间而逐渐硬化的特性(即触变硬化或触变恢复)。
国内学者通过原位测试和室内土工试验等方法对我国沿海一带软黏土的灵敏性进行了一些研究[1-4],提出了我国各地区软黏土的灵敏度和灵敏性分类,对灵敏度成因、重塑方式等对灵敏度的影响等进行了分析。此外,也有从矿物成分、微观结构等方面对我国软黏土的结构性和灵敏性进行了研究[5-6],认为软土的微结构特征、矿物成分等多方面因素造成了我国软黏土具有中等-高灵敏性和灵敏度差异。
在触变恢复研究方面,Mitchell[7]总结了前人的实验结果,最早建立了解释黏性土触变机理的微结构模型。……